Aquamet 22 Stainless Steel

Aquamet 22 Stainless Steel

Aquamet 22 Stainless Steel Chemical Composition The above tensile strength ranges are typical. If you require different please ask.
Chat Now

Product Details

Aquamet 22 Stainless Steel

Chemical Composition

ElementMin %Max %
C0.06
Si1.00
Mn4.06.0
Ni11.513.5
Cr20.523.5
S0.03
P0.04
Mo1.53.0
N0.200.40
V0.100.30
Nb/Cb0.100.30
Febal


SpecificationsDesignations

Key Features

Typical Applications

ISO 15156-3 (NACE MR0175)

W.Nr. 1.3964
UNS S20910
AWS 165

Superior corrosion resistance to type 316 stainless steel.
Good mechanical properties at ambient and sub-zero temperatures.
Does not become magnetic when cold worked or cooled to sub-zero temperatures.

Components in processing environments like:
– marine
– petroleum
– petrochemical
– fertilizer
– pulp and paper


Density

7.88 g/cm³

0.285 lb/in³

Melting Point

1415 – 1450°C

2579 – 2642°F

Coefficient of Expansion

16.2 μm/m °C (20 – 100°C)

9.0 x 10-6 in/in °F (70 – 200°F)

Modulus of Rigidity

78.9 kN/mm²

11444 ksi

Modulus of Elasticity

196.5 kN/mm²

28500 ksi


Heat Treatment of Finished Parts
Condition as supplied by Alloy Wire

Type

Temperature

Time (Hr)

Cooling

°C

°F

Annealed or Spring Temper

Stress Relieve

250

480

1

Air


Properties

Condition

Approx. tensile strengthApprox. operating temperature

N/mm²

ksi

°C

°F


Solution Annealed

700 – 1000

102 – 145

-200 to +300

-330 to +570

Spring Temper

1300 – 2200

189 – 319

-200 to +300

-330 to +570


The above tensile strength ranges are typical. If you require different please ask.


Hot Tags: aquamet 22 stainless steel, China, manufacturers, suppliers, distributor, factory, buy, price