EN 1.4318, ASTM 301LN / UNS S30153 Stainless Steel Plate

EN 1.4318, ASTM 301LN / UNS S30153 Stainless Steel Plate

EN 1.4318, ASTM 301LN / UNS S30153 Stainless Steel Plate General Characteristics 301LN/1.4318 is a low-carbon, nitrogen-alloyed alternative to 301LN/1.4318 with elevated strength, making it particularly suitable for lightweight construction applications. Typical Applications Vehicle chassis...
Chat Now

Product Details

EN 1.4318, ASTM 301LN / UNS S30153 Stainless Steel Plate

General Characteristics

301LN/1.4318 is a low-carbon, nitrogen-alloyed alternative to 301LN/1.4318 with elevated strength, making it particularly suitable for lightweight construction applications.


Typical Applications

  • Vehicle chassis


Product forms, available sizes and finishes

Flat

Product typeFinishesThicknessWidth

Cold rolled coil

2H

0,05-6,00

3-1530

Cold rolled sheet

2H

0,50-6,00

35-1530

Precision strip

2H

0,05-1,50

3-630


Chemical Composition (% by mass)


CMnCrNiMoN
Typical

0.02


17.7

6.5


0.14

ASTM A240

≤0.03

≤2.00

16.0-18.0

6.0-8.0


0.07-0.20

ASTM A666

≤0.03

≤2.00

16.0-18.0

6.0-8.0


0.07-0.20

EN 10028-7

≤0.030

≤2.00

16.50-18.50

6.00-8.00


0.10-0.20

EN 10088-2

≤0.030

≤2.0

16.5-18.5

6.0-8.0


0.10-0.20

EN 10088-4

≤0.030

≤2.0

16.5-18.5

6.0-8.0


0.10-0.20

IS 6911

≤0.03

≤2.00

16.0-18.0

6.0-8.0

≤0.70

0.07-0.20


Mechanical Properties

StandardRp0.2Rp1.0RmRockwellHB

MPa

MPa

MPa



Product type: Cold rolled coil and sheet

Typical (thickness 1 mm)

360

400

750



ASTM A240

≥ 240


≥ 550

≤ 100HRB

≤ 241

EN 10028-7

≥ 350

≥ 380

650-850



EN 10088-2

≥ 350

≥ 380

650-850



EN 10088-4

≥ 350

≥ 380

650-850



IS 6911

≥ 240


≥ 550

≤ 100HRB

≤ 241


Physical Properties

DensityModulus of elasticityThermal exp. at 100 °CThermal conductivityThermal capacityElectrical resistanceMagnetizable

kg/dm3

GPa

10-6/°C

W/m°C

J/kg°C

µΩm


7.9

200

16.0

15

500

0.73

No


Corrosion Resistance

Pitting corrosion resistanceCrevice corrosion resistance

PRE

CPT

CCT

20

<10

<0

PRE Pitting Resistant Equivalent calculated using the formula: PRE = %Cr + 3.3 x %Mo + 16 x %NCPT Corrosion Pitting Temperature as measured in the Avesta Cell (ASTM G 150), in a 1M NaCl solution (35,000 ppm or mg/l chloride ions).


CCT Critical Crevice Corrosion Temperature is the critical crevice corrosion temperature which is obtained by laboratory tests according to ASTM G 48 Method F


Standards & Approvals

The most commonly used international product standards are given in the table below.

StandardDesignation
ASTM A240/A240M

TYPE 301LN / UNS S30153

ASTM A666

TYPE 301LN / UNS S30153

EN 10028-7, PED 2014/68/EU

1.4318

EN 10088-2

1.4318

EN 10088-4

1.4318

IS 6911, AMENDMENT NO. 2

ISS 301LN


Hot Tags: en 1.4318, astm 301ln / uns s30153 stainless steel plate, China, manufacturers, suppliers, distributor, factory, buy, price